Most of the parts we print are made in one of three materials: ASA, PETG or PLA. All three are thermoplastics printed with FDM (fused deposition modelling), but they behave very differently once the part is in use. Picking the right one is the easiest way to make sure a part lasts.
This guide compares the three in plain English. If you are still unsure after reading it, tell us what the part has to do on the quote form and we will recommend a material.
The short answer
- PLA for display models, visual prototypes and indoor parts that stay cool.
- PETG for tough, functional parts used indoors or in damp conditions.
- ASA for parts that live outdoors, sit in sunlight or get warm.
ASA, PETG and PLA compared
| PLA | PETG | ASA | |
|---|---|---|---|
| Toughness | Stiff but brittle | Tough, flexes before breaking | Tough and rigid |
| Heat resistance | Low: softens around 55 to 60°C | Medium: around 70 to 80°C | High: around 95 to 100°C |
| UV and weather | Poor | Fair | Excellent |
| Moisture and chemicals | Fair | Good | Good |
| Surface detail | Excellent | Good | Good, matt finish |
| Best for | Models, fit checks, indoor parts | Brackets, clips, enclosures, jigs | Outdoor parts, car parts, housings |
Temperatures are typical softening points for the material in general. The real limit for your part also depends on its shape, wall thickness and the load it carries.
PLA: crisp detail for parts that stay indoors
PLA prints cleanly and holds fine detail, so it is a good choice for display models, figurines, architectural models and prototypes used to check size, fit and appearance. It is usually the most economical of the three.
Its weaknesses are heat and impact. A PLA part left in a car on a sunny day, or near a heat source, can soften and warp. It is also stiff rather than tough, so thin sections can snap rather than bend.
Avoid PLA for: outdoor parts, anything in a vehicle, parts near motors or electronics that run warm, and clips that need to flex.
PETG: the all-rounder for functional parts
PETG is tougher than PLA. It bends slightly before it breaks, so it copes well with knocks, vibration and parts that are fitted and removed repeatedly. It also handles damp conditions and many everyday chemicals well.
That makes it our usual recommendation for brackets, clips, mounts, electronic enclosures, jigs and fixtures. If you are not sure which material you need for a working part, PETG is often the safe starting point.
Avoid PETG for: parts that will sit in direct sunlight for years, or that get hotter than around 70°C.
ASA: built for outdoors and heat
ASA was developed for outdoor use. It resists UV light, so it does not go brittle or fade the way PLA and PETG can in long-term sunlight. It also holds its shape at higher temperatures than the other two.
We recommend ASA for garden and outdoor equipment, signage, parts for vehicles, housings that sit near warm components, and anything that has to survive the British weather. It has a slightly matt finish that suits functional parts well.
Avoid ASA for: very fine display detail, where PLA usually gives a crisper result.
Questions to ask about your part
- Will it be outdoors or in sunlight? Choose ASA.
- Will it get warm? Above around 55°C, avoid PLA. Above around 75°C, choose ASA.
- Does it need to flex, clip or take knocks? Choose PETG or ASA over PLA.
- Is it mainly about looks or checking fit? PLA is usually enough.
What about other materials?
ASA, PETG and PLA cover most jobs, but some parts need more. We also print engineering materials such as carbon fibre nylon, polycarbonate, flame-retardant polycarbonate and flexible TPU. See our materials page for the full list.
Real-world examples: which material we’d choose
| Part | Where it’s used | Our usual choice | Why |
|---|---|---|---|
| Architectural model | Indoors, on display | PLA | Crisp detail, no heat or load |
| Fit-check prototype | On the bench | PLA | Fast and economical for checking size and fit |
| Cable clip or wall bracket | Indoors, flexed when fitted | PETG | Bends slightly instead of snapping |
| Electronics enclosure | Indoors, near warm components | PETG or ASA | PETG for most cases; ASA if the inside runs warm |
| Assembly jig | Workshop, handled daily | PETG | Tough and copes with knocks |
| Garden or gate fitting | Outdoors, all year | ASA | Resists UV and weather |
| Car interior trim clip | Inside a vehicle in summer | ASA | Holds its shape when a parked car gets hot |
| Outdoor sign or housing | Direct sunlight | ASA | Won’t go brittle or fade like PLA |
Common mistakes when choosing a material
Choosing PLA for a part that lives in a car
This is the most common problem we see. A car parked in the sun gets far hotter inside than the air outside, easily beyond the point where PLA softens. Dashboard mounts, phone holders and trim clips printed in PLA can droop or warp within a single summer. ASA is the safer choice for anything in a vehicle.
Assuming stiffer means stronger
PLA feels rigid, so it’s easy to assume it’s the strongest of the three. For parts that take knocks, flex when fitted, or carry a load over time, toughness matters more than stiffness. PETG and ASA give before they break, which usually makes the part last longer.
Forgetting about sunlight
A part that works perfectly indoors can fail outside. UV light gradually breaks down PLA and, more slowly, PETG, making them brittle and faded. If a part will spend its life outdoors, ASA is worth choosing from the start.
Over-specifying the material
The opposite mistake is choosing an engineering material for a part that doesn’t need it. If a part sits indoors, takes no load and stays cool, PLA or PETG will usually do the job at a lower cost.
Does the material change the accuracy?
All three print to similar accuracy on our machines, typically ±0.2 mm, or ±0.5% on larger dimensions. Layer heights range from 0.08 mm for fine detail to 0.28 mm for faster, larger parts. Material choice affects how a part behaves in use far more than how accurately it prints. Our tolerances guide explains accuracy in more detail.
Colours and finishing
On our quote form you can choose black, white, grey or another colour. If a part needs to look more finished, we offer cosmetic paint finishing, UV laser marking for logos and labels, and threaded inserts for strong, reusable fixings.
Material checklist before you order
- Where will the part be used: indoors, outdoors or in a vehicle?
- What’s the hottest it will get?
- Does it need to flex, clip, or take knocks?
- Is it mainly for looks, for checking fit, or for real use?
- How many do you need? See our guide to what affects 3D printing cost.
Put the answers in the notes on the quote form and we’ll confirm the right material before printing.
Not sure? Ask us
Tell us what the part does, where it will be used and what it needs to survive, and we will recommend a material with your quote. Get a quote or call us on 0116 262 5737.